High Temperature Coatings for Ceramics, Glass and Quartz
Download Specs Request Quote
Quartz-Coat™ 845 applied to specialty lamp.
Ceramic-Inorganic
845
Single part, waterborne, silicon-filled, phosphate-bonded, brown-black coating for glass and quartz to
2000 °F (1093 °C). Primarily used for marking ceramic parts and coating automotive headlamps, stadium lighting and quartz vessels for the semiconductor industry. Standard viscosity is 200-400 cP; a higher viscosity coating, 845-HV, in the range of 500-800 cP is available upon request. Additional colors below are offered.
845-BLK
Jet Black
845-BLU
Cobalt-Aluminate Blue
845-GRY
Light-Gray
845-GLT
Light-Green
845-GDK
Dark-Green
845-SIL
Silver
845-WHT
White
Glass
613
Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1150 °F (620 °C).
617
Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1500 °F (816 °C).
850
Glass-ceramic filled, white reflective coating for glass and quartz to 1500 °F (816 °C).
Silicone
LC4010-BT
Aluminum-filled coating for application over black top coated headlamps to 1020 °F (550 °C).
LC4010-GL
Aluminum-filled coating for application directly over uncoated headlamps to 1020 °F (550 °C).
LC4040-SG
White reflective coating for use on mercury vapor lamps and other high temperature glass and quartz components to
1200 °F (649 °C).